Three copies of a book that had been optionally deacidified using two different procedures in 1967, and then subjected to accelerated aging, were tested again after 52 years of natural aging. Matched copies of the book Cooking the Greek Way, which had been printed in Czechoslovakia on acidic paper, were evaluated. Nonaqueous treatment of two of the copies with magnesium methoxide dissolved in chlorofluorocarbon solvent had been found in 1967 to have decreased the susceptibility to embrittlement, as evidenced by the results of the accelerated aging, followed by folding endurance tests. Retesting of the same books in 2019, after 52 years of room temperature storage, showed that the deacidification treatments had achieved the following benefits in comparison to the untreated book: (a) higher brightness; (b) higher folding endurance; (c) tensile breaking length higher in the cross-direction of the paper; (d) substantial alkaline reserve content, (e) an alkaline surface pH in the range 7.1-7.4, and (f) higher molecular mass of the cellulose. Remarkably, some of the folding endurance results matched those of unaged samples evaluated in 1967. Scanning electron micrographs showed no differences between the treated and untreated books.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.9
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据