4.2 Article

Effects of Alloy Composition and Solid-State Diffusion Kinetics on Powder Bed Fusion Cracking Susceptibility

期刊

出版社

SPRINGER
DOI: 10.1007/s11669-020-00844-y

关键词

additive manufacturing; aluminum alloy; cracking susceptibility; diffusion; laser powder bed fusion

资金

  1. Office of Naval Research [N00014-17-1-2559]
  2. CDCC Army Research Laboratory [W911NF1720172]

向作者/读者索取更多资源

The study examines the influence of solute concentration on the solidification cracking susceptibility in aluminum alloys processed by LPBF technology. It reveals a correlation between cracking susceptibility and alloy composition, indicating the significant impact of the presence of solutes on reducing the risk of solidification cracking.
Laser powder bed fusion (LPBF) has demonstrated its unique ability to produce customized, complex engineering components. However, processing of many commercial Al-alloys by LPBF remains challenging due to the formation of solidification cracking, although they are labelled castable or weldable. In order to elucidate this divergence, solidification cracking susceptibility from the steepness of the solidification curves, specifically |dT/dfS(1/2)|, as the fraction solidified nears 1 towards complete solidification, was calculated via Scheil-Gulliver model as a function of solute concentration in simple binary Al-Si, Al-Mg, and Al-Cu systems. Introduction of diffusion in solid into Scheil-Gulliver model resulted in a drastic reduction in the cracking susceptibility (i.e., reduction in the magnitude of |dT/dfS(1/2)|) and a shift in the maximum |dT/dfS(1/2)| to higher concentrations of solute. Overall, the calculated solidification cracking susceptibility correlated well with experimental observation made using LPBF AA5083 (e.g., Al-Mg) and Al-Si binary alloys with varying Si concentration. Cracking susceptibility was found to be highly sensitive to the composition of the alloy, which governs the variation of |dT/dfS(1/2)|. Furthermore, experimental observation suggests that the contribution of diffusion in solids to reduce the cracking susceptibility can be more significant than what is expected from an instinctive assumption of negligible diffusion and rapid cooling typically associated with LPBF.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据