4.7 Article

Poly(butylene succinate-ran-ε-caprolactone) copolyesters: Enzymatic synthesis and crystalline isodimorphic character

期刊

EUROPEAN POLYMER JOURNAL
卷 95, 期 -, 页码 795-808

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.eurpolymj.2017.05.002

关键词

Poly(epsilon-caprolactone); Poly(butylene succinate); Random copolymers; Enzymatic synthesis; ROP; Cyclic oligomers; Isodimorphism

资金

  1. Ministerio de Economia y Competitividad (MINECO) of Spain [MAT2012-38044-C03-03, MAT2016-77345-C3-1-P]
  2. Agencia de Gestio d'Ajuts Universitaris i de Recerca (AGAUR) (Catalonia, Spain) [2009SGR1469]
  3. Spanish Ministry (MINECO) [MAT2015-63704-P]
  4. Eusko Jaurlaritza (Basque Government) [IT-654-13]
  5. CNPq (National Research Council) Brazil
  6. POLYMAT Basque Center for Macromolecular Design and Engineering
  7. Consejo Nacional de Ciencia y Tecnologia (CONACYT) (Mexico)
  8. [UPV/EHU Infrastructure: INF 14/38]
  9. [MINECO/FEDER: SINE 130I001726XV1/]
  10. [UNPV13-4E-1726]
  11. [MINECO MAT2014-53437-C2-P]

向作者/读者索取更多资源

In this paper, the preparation of PBS-ran-PCL copolyesters by enzymatic ring opening polymerization is presented for the first time. The copolyesters were produced in a wide composition range and free of metallic contaminants, so they may be regarded as potential biomaterials. The copolymers have been characterized by proton and carbon nuclear magnetic resonance OH and C-13 NMR), gel permeation chromatography (GPC), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), polarized light optical microscopy (PLOM) and wide angle X-ray scattering (WAXS). The PBS-ran-PCL copolyesters were able to crystallize in the entire composition range and displayed a pseudo-eutectic region. Most copolymers away from the pseudo-eutectic region exhibited a single crystalline phase (PBS-rich or PCL-rich crystalline phase), while within the pseudo-eutectic region the copolymers were double crystalline. Observations by PLOM, during isothermal crystallization showed that both nucleation density and spherulitic growth rate of the copolyesters are determined by the component that constitutes the majority phase. WAXS studies revealed that d spacings of selected crystallographic planes depend on composition. Therefore, both DSC and WAXS results suggest that the copolymers are probably isodimorphic, as the PBS-rich crystalline phase may contain small inclusions of PCL co-units, while the PCL-rich crystalline domains may also contain a minor quantity of PBS co-units inside.