Adding 10 mM KPF6 to the 1 M LiPF6 in ethylene carbonate/dimethyl carbonate electrolyte of symmetrical Li vertical bar Li cells eliminated the growth of dendrites at 0.5 mA cm(-2) current density and massively reduced, but did not eliminate, the growth of dendrites at 2.5 mA cm-(2.) The added KPF6 increased the fraction of inorganic salts in the solid electrolyte interface, making it thinner and more Li+ conductive. It overcame the growth of dendrites resulting from inadequate nucleation density but not dendrite growth into the depletion layer, which scales with the layer's thickness, i.e., the current density.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据