4.7 Article

Photocatalytic degradation of perfluorooctanoic acid (PFOA) via MoS2/rGO for water purification using indoor fluorescent irradiation

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.jece.2022.108466

关键词

Graphene oxide; Composites; Metal disulphide; Photocatalytic degradation; PFOA; Sustainable water treatment

资金

  1. Fundamental Research Grant Scheme by Ministry of Higher Education Malaysia [FRGS/1/2018/STG01/UITM/02/1]
  2. Universiti Teknologi MARA Malaysia [600-RMC/GIP 5/3 (103/2022)]

向作者/读者索取更多资源

This study successfully synthesized MoS2/rGO nanocomposites and confirmed the effective incorporation of MoS2 into GO structures using various characterization methods. MoS2/rGO-15 exhibited superior performance in the photocatalytic degradation of PFOA.
The current investigation focussed on the facile synthesis of MoS2/rGO nanocomposite with different weight percentages of MoS2 (1%, 5% and 15% w.r.t. to rGO) prepared via hydrothermal methods. The effective incorporation of MoS2 on the GO structures was substantially confirmed via various characterization tools via attenuated total reflectance-Fourier transform infrared (ATR-FTIR), ultraviolet-visible spectroscopy(UV-VIS), scanning electron microscope (SEM), transmision electron microscope (TEM), x-ray diffractometry (XRD), Raman spectroscopy, thermogravimetric analysis (TGA), surface area and pore analyzer, zeta potential and x-ray photoelectron spectroscopy (XPS). The nanocomposites were applied as photocatalysts to degrade per-fluorooctanoic acid (PFOA) using a photoreactor equipped with an 18-watt fluorescent lamp. MoS2/rGO-15 showed superior photocatalytic properties for degrading PFOA, with kinetic rate constant k = 0.0758 min(-1), and t (1/2) = 1.524 h under fluorescent light evaluated by using the Langmuir-Hinshelwood (L-H) model. The reusability studies indicated that the MoS2/rGO-15 composites can be reused for up to six cycles. Real water sample analysis revealed that MoS2/rGO-15 is efficient in degrading PFOA in a river water sample with a 77% degradation percentage. Thus, this research proposed a sustainable solution for photocatalytic degradation of PFOA in water purification under fluorescent light.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据