Analysis of hole quality in drilling GLARE fiber metal laminates

期刊

COMPOSITE STRUCTURES
卷 123, 期 -, 页码 350-365

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.compstruct.2014.12.056

关键词

Drilling; GLARE; Fiber metal laminates; Thrust force; Acoustic emission; C-scan

资金

  1. National Centre for Aerospace Innovation and Research (NCAIR(TM))

向作者/读者索取更多资源

Glass laminate aluminium reinforced epoxy (GLARE) is an advanced aircraft material because of its excellent fatigue crack resistance, high impact strength, high strength-to-weight ratio and high stiffness-to-weight ratio. While drilling on composite/metal stacks has been investigated, the drilling of GLARE, which consists of several alternate thin layers of aluminium and composites, has not been addressed separately in the open literature. The focus of present experimental work is to understand the cutting mechanism and relative effect of cutting parameters and tool geometry on the delamination and burr formation during drilling of GLARE. Thrust force, torque and acoustic emission (AE) signals were acquired for analyzing the cutting mechanism, burr and delamination formation. Also, several measurements of burrs, delamination and hole size were taken in order to understand the hole quality. It has been observed that, 2-fluted drill is the best out of four different geometries used, giving zero delamination and acceptable burr formation followed by the 4-faceted drills. The conventional 3-fluted and 8-faceted drills that are otherwise superior for drilling of fiber reinforced plastics (FRP) composites, performed poorly in drilling of the GLARE laminates. Analyzing the processing parameters, feed again has a dominant role in controlling delamination and burr formation than speed. (C) 2015 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据