Evaluation of heat resistance of SiC-based ceramic fibers via in situ elastic modulus and electrical conductivity measurement at elevated temperatures

期刊

JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
卷 44, 期 2, 页码 802-814

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.jeurceramsoc.2023.10.008

关键词

Silicon carbide; Ceramic fiber; Mechanical property; Physical property; Microstructural analysis

向作者/读者索取更多资源

The in situ thermal stability of SiC-based ceramic fibers was investigated, and the third-generation fibers showed excellent stability at temperatures up to 1800 degrees C.
SiC-based ceramic fibers have numerous applications as reinforcement materials. Herein, the in situ thermal stability of four types of SiC-based ceramic fibers from three generations was investigated in terms of elastic modulus and electrical conductivity at temperatures up to 1800 degrees C in a vacuum under low pressure (<10(-4)Pa). A specific tensile test device (MacaSiC) for single fibers was used. Mechanical and physical properties were monitored during heating and cooling at 1200, 1500, and 1800 degrees C for 10 min. Fibers exposed at 1200, 1500, and 1800 degrees C for 10 min were evaluated by measuring tensile strength retention, and correlating them with fiber crystallinity and microstructural evolution. Third-generation fibers exhibited excellent thermal stability at temperatures up to 1800 degrees C. The strength degradation of the third-generation SiC fibers was associated with the enlargement of apparent beta-SiC crystallites and carbonization caused by the release of Si in the annular region of the fibers.