A particle-scale study of the triaxial compression behavior of methane hydrate-bearing sands

期刊

ACTA GEOTECHNICA
卷 -, 期 -, 页码 -

出版社

SPRINGER HEIDELBERG
DOI: 10.1007/s11440-023-02043-8

关键词

Discrete element method; Hydrate distribution; Mechanical properties; Methane hydrate-bearing sands; Triaxial compression tests

向作者/读者索取更多资源

This paper combines triaxial compression tests and numerical simulations using discrete element method (DEM) to study the mechanical properties of methane hydrate-bearing sands (MHBS) at the particle scale. The study investigates the effects of hydrate saturation, cementation network, and hydrate spatial distribution on the mechanical behavior of MHBS samples. The results provide insights into the unique mechanical properties and failure mechanisms of MHBS.
Macroscopic geomechanical properties of methane hydrate-bearing sands (MHBSs) have attracted much scholarly attention. But the associated particle-level mechanisms often rely on assumptions. In this paper, triaxial compression tests and numerical simulations using discrete element method (DEM) are combined to study the unique mechanical properties of MHBS at the particle scale. The triaxial compression tests understand the basic mechanical properties of MHBS, and the experiments results are used for DEM modeling and parameter calibration. Small cementing particles are used to simulate methane hydrate, showing dispersion and coalescence distributions in sediments to simulate different hydrate spatial distributions. The simulation results show that in MHBS samples, the increasing hydrate saturation enhances the cementation network as well as the hydrate-related micro-force chains, and the particles in the cementation network jointly share the loading. The hydrate cementation is restricted by the high effective confining pressure as the cementation network was subjected to an ultimate strength. For hydrate cementation failure, the high effective confining pressure increases the proportion of shear breakage, but tensile breakage is the dominant failure form. The sample with hydrate coalescence distribution behaves strain hardening, while the sample with hydrate dispersion distribution yields later and shows strain softening with a higher peak strength. Finally, the stress-induced anisotropy in microstructure fabrics is observed, and the development of radial fabrics is hindered by hydrates, especially the coalesced hydrates.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据