Microstructural Evolution and Mechanical Properties of Ti2AlNb/GH99 Superalloy Brazed Joints Using TiZrCuNi Amorphous Filler Alloy

期刊

AEROSPACE
卷 10, 期 1, 页码 -

出版社

MDPI
DOI: 10.3390/aerospace10010073

关键词

intermetallics; dissimilar alloys brazing; interfacial microstructure; fracture

向作者/读者索取更多资源

The dissimilar materials brazing of Ti2AlNb alloy to GH99 superalloy is of great importance in the aerospace field. The interfacial structures and properties of the joints were investigated under different brazing temperatures and times. The interfacial microstructure was influenced by diffusion and reaction between the filler alloy and the parent metal. The maximum shear strength of the joints was found to be approximately 216.2 MPa when brazed at 1000 degrees C for 8 min.
Dissimilar materials brazing of Ti2AlNb alloy to GH99 superalloy is of great pragmatic importance in the aerospace field, especially the lightweight space aircraft components manufacturing. In this work, TiZrCuNi amorphous filler alloy was used as brazing filler, and experiments were carried out at different brazing temperatures and times to investigate the changes in interfacial structures and properties of the joints. The typical interfacial microstructure was Ti2AlNb alloy/B2/beta/Ti2Ni (Al, Nb) + B2/beta + (Ti, Zr)(2)(Ni, Cu) + (Ti, Zr)(Ni, Cu)/(Cr, Ni, Ti) solid solution + (Ni, Cr) solid solution/GH99 superalloy when being brazed at 1000 degrees C for 8 min. The interfacial microstructure of the joints was influenced by diffusion and reaction between the filler alloy and the parent metal. The prolongation of brazing process parameters accelerated the diffusion and reaction of the liquid brazing alloy into both parent metals, which eventually led to the aggregation of (Ti, Zr)(2)(Ni, Cu) brittle phase and increased thickness of Ti2Ni (Al, Nb) layer. According to fracture analyses, cracks began in the Ti2Ni (Al, Nb) phase and spread with it as well as the (Ti, Zr)(2)(Ni, Cu) phase. The joints that were brazed at 1000 degrees C for 8 min had a maximum shear strength of similar to 216.2 MPa. Furthermore, increasing the brazing temperature or extending the holding time decreased the shear strength due to the coarse Ti2Ni (Al, Nb) phase and the continuous (Ti, Zr)(2)(Ni, Cu) phase.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据