Passivating electron contact based on highly crystalline nanostructured silicon oxide layers for silicon solar cells

期刊

SOLAR ENERGY MATERIALS AND SOLAR CELLS
卷 158, 期 -, 页码 2-10

出版社

ELSEVIER
DOI: 10.1016/j.solmat.2016.06.040

关键词

Surface passivation; Passivating contact; Nanostructure; Silicon oxide; Nanocrystalline; Microcrystalline; Poly-silicon; Crystallization; Raman; Transmission line measurement; Phosphorous diffusion

向作者/读者索取更多资源

We present a novel passivating contact structure based on a nanostructured silicon-based layer. Traditional poly-Si junctions feature excellent junction characteristics but their optical absorption induces current losses when applied to the solar cell front side. Targeting enhanced transparency, the poly-Si layer is replaced with a mixed-phase silicon oxide/silicon layer. This mixed-phase layer consists of an amorphous SiOx matrix with incorporated Si filaments connecting one side of the layer to the other, and is referred to as nanocrystalline silicon oxide (nc-SiOx) layer. We investigate passivation quality, measured as saturation current density, and nanostructural changes, characterized by Raman spectroscopy and transmission electron microscopy, carefully studying the influence of annealing dwell temperature. Excellent surface passivation on n-type and also p-type wafers is shown. An optimum annealing temperature of 950 degrees C is found, resulting in a saturation current density of 8.8 fA cm(-2) and 11.0 fA cm(-2) for n-type and p-type wafers, respectively. Even before forming gas annealing, emitter saturation current densities of 27.9 fA cm(-2) (n+/n junction) and 32.0 fA cm(-2) (n+/p junction) are reached. Efficient current extraction is presented with specific contact resistivities of 86 m Omega cm(2) on n-type wafer and 19 m Omega cm(2) on p-type wafers, respectively. High-resolution transmission electron microscopy reveals that the layer stack consists of intermixed SiOx and Si phases with the Si phases being partly crystalline already in the as-deposited state. Thermal annealing at temperatures >= 850 degrees C further promotes crystallization of the Si-rich regions. The addition of the SiOx phase enhances the thermal stability of the contact and should allow to tune the refractive index and improve transparency, while still providing efficient electrical transport through the crystalline Si phase, which extends throughout almost the entire contact. (C) 2016 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据