4.6 Article

Achieving highly-enhanced UV photoluminescence and its origin in ZnO nanocrystalline films

期刊

OPTICAL MATERIALS
卷 58, 期 -, 页码 382-389

出版社

ELSEVIER
DOI: 10.1016/j.optmat.2016.05.008

关键词

ZnO; UV-photoluminescence; DC-sputtering; Raman; Native defects; Annealing

资金

  1. U.S. Department of Energy, Office of Basic Energy Science, Division of Materials Science and Engineering [DE-FG02-07ER46386]

向作者/读者索取更多资源

ZnO is an efficient luminescent material in the UV-range similar to 3.4 eV with a wide range of applications in optical technologies. Sputtering is a cost-effective and relatively straightforward growth technique for ZnO films; however, most as-grown films are observed to contain intrinsic defects which can significantly diminish the desirable UV-emission. In this research the defect dynamics and optical properties of ZnO sputtered films were studied via post-growth annealing in Ar or O-2 ambient, with X-ray diffraction (XRD), imaging, transmission and Urbach analysis, Raman scattering, and photoluminescence (PL). The imaging, XRD, Raman and Urbach analyses indicate significant improvement in crystal morphology and band-edge characteristics upon annealing, which is nearly independent of the annealing environment. The native defects specific to the as-grown films, which were analyzed via PI, are assigned to Zn-i related centers that luminesce at 2.8 eV. Their presence is attributed to the nature of the sputtering growth technique, which supports Zn-rich growth conditions. After annealing, in either environment the 2.8 eV center diminished accompanied by morphology improvement, and the desirable UV-PL significantly increased. The 02 ambient was found to introduce nominal O-i centers while the Ar ambient was found to be the ideal environment for the enhancement of the UV-light emission: an enhancement of similar to 40 times was achieved. The increase in the UV-PL is attributed to the reduction of Zn-i-related defects, the presence of which in ZnO provides a competing route to the UV emission. Also, the effect of the annealing was to decrease the compressive stress in the films. Finally, the dominant UV-PL at the cold temperature regime is attributed to luminescent centers not associated with the usual excitons of ZnO, but rather to structural defects. (C) 2016 The Authors. Published by Elsevier B.V.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据