The objective of this study was to develop a yttria-stabilized zirconia catalyst-supported nickel (Ni/YSZ) with high tolerance to coke deposition during methane steam reforming (MSR). The Ni/YSZ catalyst prepared by an electroless plating method (Ni(el)/YSZ) exhibited better stability during the MSR than did the catalyst prepared by a conventional impregnation method (Ni(im)/YSZ). Additionally, the amount of coke deposition on the Ni(el)/YSZ catalyst was lower than that on the Ni(im)I YSZ catalyst. By thermal treating the Ni(el)YSZ catalyst in a nitrogen atmosphere before the reforming reaction, a further decrease in the deposited coke amount was observed. In particular, the deposited coke was not detected at all over the Ni(el)/YSZ catalyst pretreated at 1073 K for 2 h.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据