4.6 Article

Surface Magnesium Substitution at Spinel Lithium Manganate 8a Tetrahedral Sites for Suppressed Manganese Dissolution and Enhanced Cycle Stability

期刊

ACS ENERGY LETTERS
卷 8, 期 10, 页码 4278-4286

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsenergylett.3c01560

关键词

-

向作者/读者索取更多资源

Surface magnesium ion substitution significantly suppresses the surface evolution and manganese dissolution of LiMn2O4, solving the surface degradation issue that has lasted for decades. This study introduces a strategy of surface magnesium doping through ALD coating and annealing, resulting in high capacity retention after 250 cycles.
Surface degradation induced by the dissolution of manganese is a major failure mechanism that has hampered the large-scale adoption of spinel LiMn2O4 cathode material for decades. Although modifications based on restraining manganese disproportionation reactions have received much attention, many of these methods may sacrifice batteries' specific capacity and rate capability. Here, we present a strategy that surface-populated magnesium ion substitution at 8a tetrahedral sites in LiMn2O4 could significantly suppress spinel surface evolution and Mn dissolution during cycling. With a total trace amount of magnesium surface doping (0.3 wt %) introduced by ALD coating and annealing, the LiMn2O4 cathode shows a capacity retention of 98.6% after 250 cycles. This study reveals the role of atomic doping site selection and the significance of the electrode materials' surface stability at the charged state.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据