Laser powder bed fusion; Al-12Si; Defects; Microstructure; Mechanical properties

向作者/读者索取更多资源

Laser power and scan speed are crucial parameters in laser powder bed fusion, affecting defects and microstructures. By adjusting the parameter combination, the performance and microstructure of the samples can be improved.
The laser power and scan speed are significant processing parameters influencing the defects and microstructures due to affecting the thermal state within the melt pool during laser powder bed fusion (LPBF). To this end, these process parameter combinations under a constant laser energy density are correlated with defects (balling phenomenon and pores) and microstructures (melt pool arrangement and cell morphology). Setting the parameter combination (laser power and scan speed are 200 W and 910 mm/s, respectively) yields large balling droplets (average size of 150 mm) due to the relatively high melt viscosity resulting from the low melt pool temperature. In this case, a limited surface tension difference acting on a liquid surface cannot provide sufficient driving forces against viscous drags to promote the efficient spreading of the molten alloy. Cavity regions are formed between the large balling droplets and the previous layer, forming lack-of -fusion pores. By increasing the laser power and scan speed gradually, samples with relative densities greater than 99.5% are produced. This phenomenon can be attributed to the increases in laser power and scan speed, which improves the spreading ability of the molten alloy. With increasing laser power and scan speed, the cell size decreases (from 0.51 mm to 0.42 mm) because of the increase in the cooling rate. The sample (laser power and scan speed are 350 W and 1590 mm/s, respectively) has the highest performance (310 MPa yield strength, 470 MPa ultimate tensile strength, and 6.6% fracture strain) due to its highest relative density (greater than 99.5%) and fine microstructure (average cell size of 0.45 mm). All four samples exhibit anisotropic mechanical properties resulting from the combination of the melt pool boundary and lack-of-fusion pores.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据