This study discusses the manufacturing of porous ceramic granules using inexpensive silica source and a biopolymer cross-linked by ion exchange. The results showed that porous diatomite granules with high sphericity could be successfully obtained by optimizing the dispersion conditions. The manufacturing process also resulted in hierarchically porous diatomite granules with high sphericity, acceptable compressive strength, and porosity features, making them suitable for catalytic or adsorption applications.
The proper application of millimeter-sized spherical porous ceramic supports in catalytic operations relies on their ease of handling, convenient separation, recyclability, high-catalyst-solid loading, and the optimum mass transfer of reactants and products. However, common granulation techniques of spherical carriers entail complex liquid-phase-based processes under severe conditions and the use of toxic or expensive reagents. The present study discusses the manufacturing of porous ceramic granules derived from an inexpensive silica source (diatomite, solid network) and a biopolymer cross-linked by ion exchange (sodium alginate, patterning structure). The results indicated that, with fixed granulation conditions, porous diatomite granules with a sphericity of approximately 0.9 could be successfully obtained by optimization of the diatomite/sodium alginate dispersion to a 30.07 wt.% solid content and 1560 mPa.s viscosity (at similar to 0.3 s(-1)). Moreover, the described manufacturing process was proven effective in developing hierarchically porous diatomite granules that were heat-treated at 1200 degrees C with high sphericity (similar to 0.9), acceptable compressive strength (5.17 +/- 0.31 MPa), and porosity features (total porosity: 69.0 +/- 2.9%, macropore size: 2.777 mu m, mesopore size: 35.34 nm), establishing them as well-matched support materials for either catalytic or adsorption applications.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据