This study developed a non-destructive prestressed strengthening solution for steel beams using adhesively bonded Fe-SMA strips. The behavior of the Fe-SMA-to-steel bonded joints was investigated, and an effective bond length of approximately 120 mm was determined. A strengthening solution for a 5.3 m span steel I-beam was designed and experimentally tested, demonstrating reliable performance under service loads.
This study entails the development of a non-destructive prestressed strengthening solution for steel beams using adhesively bonded memory-steel (also known as iron-based shape memory alloy, Fe-SMA) strips. The Fe-SMA strip is activated via heating and subsequent cooling to generate prestress, while the two ends of the Fe-SMA strip are adhesively bonded as anchorages. The behavior of the Fe-SMA-to-steel bonded joints was investigated through lap-shear tests, from which an effective bond length of approximately 120 mm was determined. Subsequently, a strengthening solution for a 5.3 m span steel I-beam was designed based on finite element analysis. A 4200 mm x 100 mm x 1.5 mm Fe-SMA strip was bonded to the bottom of the steel beam with a bond length of three times the effective bond length, and a two-step activation strategy using torches was proposed. Furthermore, the designed strengthening solution was experimentally tested. With activation to the target temperature of 240 degrees C, the Fe-SMA developed a prestress level of approximately 280 MPa. A series of static and fatigue four-point bending tests were conducted. After 3 million cycles of fatigue loading, no debonding or degradation was observed for the adhesively bonded Fe-SMA-strengthened specimen; this demonstrated the reliable performance of the strengthening solution under service loads.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据