This paper presents a strategy for removing excess cured areas caused by light scattering in order to improve the forming accuracy and speed of ceramic parts.
Stereolithography technology shows great potential for manufacturing ceramic parts with complex structures. However, it seems difficult to achieve both high forming accuracy and speed. Excess cured areas caused by light scattering is one of the main reasons for the degradation of accuracy. This paper presents a special strategy to remove the excess cured areas by utilizing the shear stress that is generated during the forming process. By adjusting the feeding speed, feeding height, feeding temperature and their combinations, the shear stress can be controlled to be beneficial. The relative forming error greatly decreased by 51.66% for small features. As the feeding speed was increased to 3 or 4 times, the forming accuracy of the structures on different surfaces was increased to 9 times or 2.8 times. This work provides a simple, general and low-cost method for rapid and highaccuracy manufacturing of ceramic parts, especially for those with small structural features.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据