4.5 Article

The Effect of Forging and Heat Treatment Variables on Microstructure and Mechanical Properties of a Re-Bearing Powder-Metallurgy Nickel Base Superalloy

期刊

METALS
卷 13, 期 6, 页码 -

出版社

MDPI
DOI: 10.3390/met13061110

关键词

nickel base superalloy; powder metallurgy; microstructure; forging; heat treatment; tensile properties; creep properties

向作者/读者索取更多资源

The effects of forging and heat treatment variables on microstructure evolution and mechanical properties were studied in a Re-bearing nickel base superalloy prepared via powder metallurgy. The properly balanced mechanical properties were reached for a certain grain size of the alloy.
In our previous works, the effects of forging and heat treatment variables on microstructure evolution and mechanical properties have been studied for an ingot-metallurgy Re-bearing nickel base superalloy. To overcome the issues associated with the production of large-scale ingots and fine-grained workpieces, in the present work, the effect of hot forging and heat treatment variables was studied in a Re-bearing nickel base superalloy prepared via powder metallurgy. The purpose of the study was to reach the properly balanced mechanical properties for the potential use of the superalloy as a disc material. The initial as-HIPed workpieces were subjected to different hot forging and post-forging heat treatment or only to heat treatment (no forging). For the processed workpieces, the recrystallization behavior, size, morphology and volume fraction of & gamma;& PRIME; precipitates were evaluated by scanning electron microscopy followed by a study of mechanical properties. The most properly balanced mechanical properties (strength, ductility, creep resistance and creep rupture lifetime) were reached for the & gamma; grain size of d(& gamma;) & AP; 13.6 & mu;m. A finer and coarser & gamma; grain size (down to d(& gamma;) & AP; 2.6 and up to d(& gamma;) & AP; 37.5 & mu;m) even when superimposed with a higher volume fraction of dispersed secondary & gamma;& PRIME; precipitates (in the case of d(& gamma;) = 27-37.5 & mu;m) was associated with worse mechanical properties.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据