Evolution of Microstructures, Texture and Mechanical Properties of Al-Mg-Si-Cu Alloy under Different Welding Speeds during Friction Stir Welding

期刊

METALS
卷 13, 期 6, 页码 -

出版社

MDPI
DOI: 10.3390/met13061120

关键词

aluminium alloy; EBSD; GND; texture; mechanical properties

向作者/读者索取更多资源

The effects of different welding speeds on the microstructures and mechanical properties of Al-0.75Mg-0.75Si-0.8Cu alloys were investigated. The results showed that the welded joint formed different zones and exhibited various textures. The NZ underwent dynamic recrystallisation and had the smallest grain size and best mechanical properties at a welding speed of 125 mm/min.
The effects of different welding speeds on the microstructures and mechanical properties of Al-0.75Mg-0.75Si-0.8Cu alloys were investigated using optical metallographic microscopy (OM), X-ray diffraction (XRD) analysis, an ETM105D electronic universal testing machine and field emission electron microscopy (SEM). The results reveal that during the friction stir welding process, the welded joint forms the base material (BM), heat-affected zone (HAZ), thermomechanically affected zone (TMAZ) and nugget zone (NZ), under the action of shear force and friction heat. The textures present in the BM are mainly C ({001}<100>) recrystallised cubic texture and P({110}<112>) recrystallised texture, Goss (G) texture, brass (B) texture and {112}<110> rotating copper texture. The organisation of the NZ undergoes dynamic recrystallisation, forming fine isometric crystals with large angular grain boundaries, accounting for more than 75% of the total. The geometrically necessary dislocations (GNDs) in the NZ grow as the welding speed rises. Moreover, {111}<1<(1)over bar>0> and {(1) over bar 11}< 1 10> shearing textures, {001}<110> recrystallisation textures and fibre textures are mainly present in NZs. The average grain size in the NZ was the smallest, and the mechanical properties were the best at a welding speed of 125 mm/min. The grain size and the tensile strength and elongation of the NZ were 2.945 mu m, 200.7 MPa and 12.7% for the joint at a welding speed of 125 mm/min, respectively.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据