This study investigated the influence of interface structure on the hydrothermal aging of four carbon fiber reinforced epoxy resin composites (CFRPs). The results showed that CF-COOH-EP had the highest moisture absorption due to the presence of hydrophilic groups in the interface. The addition of Mxene nanosheets helped reduce the moisture absorption rate of CF-COOH/MXene/EP and CF-CONH-MXene-EP, making it similar to that of CF/EP. The interface structure also had an impact on the inter-laminar shear strength (ILSS) changes during aging, with CF-COOH-EP showing the fastest aging and lowest ILSS retention rate, while CF-CONH-MXene-EP exhibited the highest ILSS after aging.
Four carbon fiber reinforced epoxy resin composites (CFRPs), CF/EP, CF-COOH-EP, CF-COOH/MXene/EP and CF-CONH-MXene-EP, were prepared and subjected to hydrothermal aging experiments at 55 degrees C. The changes in structure and mechanical property of these CFRPs, having different interface, before and after the aging were investigated to explore the influence of interface structure on hydrothermal aging of CFRPs. CF-COOH-EP has the highest moisture absorption because of a large number of hydrophilic groups in the interface. The Mxene nanosheets help reduce the moisture absorption rate and equilibrium moisture absorption of CFRPs CF-COOH/ MXene/EP and CF-CONH-MXene-EP is similar to that of CF/EP. The aging results in decreases of storage modulus and temperature at maximum tan delta, but the different interface structures show little influence on them. The inter -laminar shear strength (ILSS) presents a fast decline in the early aging and a gradual decrease at the following stage. The interface structure has an influence on the hydrothermal aging of the CFRPs and results in different ILSS changes. Among the four CFRPs, CF-COOH-EP presents the fastest hydrothermal aging corresponding the lowest ILSS retention rate and CF-CONH-MXene-EP keeps the highest ILSS after aging exhibiting the highest reliability.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据