The veneering porcelain sintered on zirconia is widely used in dental prostheses, but repeated mechanical loadings may cause a fracture such as edge chipping or delamination. In order to predict the crack initiation angle and fracture toughness of zirconia/veneer bilayered components subjected to mixed mode loadings, the accuracy of a new and traditional fracture criteria are investigated. A modified maximum tangential stress criterion considering the effect of T-stress and critical distance theory is introduced, and compared to three traditional fracture criteria. Comparisons to the recently published fracture test data show that the traditional fracture criteria are not able to properly predict the fracture initiation conditions in zirconia/veneer bi-material joints. The modified maximum tangential stress criterion provides more accurate predictions of the experimental results than the traditional fracture criteria. (C) 2015 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据