CVD-SiC coated and uncoated ceramic matrix composites (C-f/SiC and SiCf/SiC) were joined to their counterparts with a pre-sintered Ti3SiC2 foil using Spark Plasma Sintering. For the first time pre-sintered Ti3SiC2 foil was used as a joining filler. The joining parameters were carefully selected to avoid the decomposition of Ti3SiC2 and the reaction between the joining filler and the CVD-SiC coating, which would have deteriorated the oxidation protective function of the coating. Conformal behaviour of the Ti3SiC2 foil during the diffusion joining and the infiltration of the joining filler into the surface cracks in the CVD beta-SiC coating allowed the filler to be more integrated with the matrix material. While diffusion bonding occurred during joining of the coated composites, a combination of both solid-state reaction and diffusion bonding was observed for the uncoated C-f/SiC composites. This produced the lower shear strength (19.1 MPa) when compared to the diffusion bonded CVD-SiC coated C-f/SiC (31.1 MPa). Crown Copyright (C) 2016 Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据