4.8 Article

Activity-Stability Trends of the Sb-SnO2@RuOX Heterostructure toward Acidic Water Oxidation

期刊

ACS APPLIED MATERIALS & INTERFACES
卷 15, 期 12, 页码 15332-15343

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsami.2c21017

关键词

RuOx; heterostructure; interface stability; electrochemical; water oxidation

向作者/读者索取更多资源

This study evaluates the activity and stability of in situ crystallized antimony-doped tin oxide (Sb-SnO2)@RuOx heterostructure nanosheets (NSs) for acidic water oxidation. The catalyst prepared by atomic layer deposition and heat treatment exhibits comparable activity but longer stability than the ex situ catalyst. The controlled interface stability of heterostructure catalysts plays a significant role in enhancing oxygen evolution reaction (OER) activity and stability.
Accomplishments of enhanced activity and durability are a major concern in the design of catalysts for acidic water oxidation. To date, most studied supported metal catalysts undergo fast degradation in strongly acidic and oxidative environments due to improper controlling of the interface stability caused by their lattice mismatches. Here, we evaluate the activity-stability trends of in situ crystallized antimony-doped tin oxide (Sb-SnO2)@RuOx (Sb-SnO2@RuOx) heterostructure nanosheets (NSs) for acidic water oxidation. The catalyst prepared by atomic layer deposition of a conformal Ru film on antimony-doped tin sulfide (Sb-SnS2) NSs followed by heat treatment highlights comparable activity but longer stability than that of the ex situ catalyst (where Ru was deposited on Sb-SnO2 followed by heating). Air calcination for in situ crystallization allows the formation of hierarchical mesoporous Sb-SnO2 NSs from as-prepared Sb-SnS2 NSs and parallel in situ transformation from Ru to RuOx, resulting in a compact heterostructure. The significance of this approach significantly resists corrosive dissolution, which is justified by the enhanced oxygen evolution reaction (OER) stability of the catalyst compared to most of the state-of-the-art ruthenium-based catalysts including Carbon@RuOx (which shows similar to 10 times higher dissolution) as well as Sb-SnO2@Com. RuOx and Com. RuO2. This study demonstrates the controlled interface stability of heterostructure catalysts toward enhancing OER activity and stability.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据