This study used 3D surface scanning and subtraction radiography to examine the dimensional changes of endodontic sealers over 18 months. The results showed that Apexit Plus had the largest dimensional changes, followed by TubliSeal EWT and BioRoot RCS, while AH Plus remained stable throughout 18 months.
Objectives: To examine the dimensional changes of endodontic sealers during 18 months using three-dimensional (3D) surface scanning and subtraction radiography in a novel in vitro sealer-extrusion model. Material and Methods: Fifty endodontically instrumented acrylic teeth were randomly allocated to five groups (n = 10) filled with Apexit Plus, AH Plus, BioRoot RCS, TubliSeal EWT, and gutta-percha (control). Freshly mixed sealers were intentionally extruded during obturation. All teeth were immersed in a physiologic solution for up to 18 months. Blinded 3D surface scans (resolution: similar to 10 mu m) and digital radiographs of the teeth were obtained at baseline (immediately after obturation); and then after 1 week, and at 1, 3, and 18 months. For blinded assessment of sealer dimensional change, 3D models and radiographs were superimposed using specific software. Volumetric differences, root mean square (RMS), and area change from subtraction radiography measured at each period within each sealer group were thereafter calculated. Repeated measures analyses were done with Bonferroni adjustment for multiple comparisons; standard errors, p values, and 95% confidence intervals (CI) were reported. Results: Analyses of the volumetric data confirmed significant, progressive material loss for Apexit Plus when compared to the other investigated sealers or the control group (p <= 0.02). Immersion period significantly influenced the volumetric dimensional changes of Apexit Plus already after 1 month (p < 0.01). For TubliSeal EW, the effect of the immersion period on the dimensional changes was noted after immersion for 3 months (p <= 0.02), while for BioRoot RCS this was evident only at 18 months (p < 0.01). Same trends were noted for the RMS data, whereas progressive dimensional changes using subtraction radiography only revealed significant changes for Apexit Plus (p = 0.01). Conclusions: The largest dimensional changes were shown by Apexit Plus, followed by Tubliseal EWT and BioRoot RCS. AH Plus remained stable throughout 18 months.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据