Molecular Weight Controls Interactions between Plastic Deformation and Fracture in Cold Spray of Glassy Polymers

期刊

ACS OMEGA
卷 -, 期 -, 页码 -

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsomega.2c06617

关键词

-

向作者/读者索取更多资源

Polymer cold spray is a novel manufacturing process that allows for the deposition of uniform polymer coatings without the need for solvents or high temperatures. This study investigates the interplay between shear instability and fracture in the deposition of glassy thermoplastics, using a hybrid experimental-computational approach. The results demonstrate that the adhesion mechanisms depend strongly on the molecular weight of the sprayed particles, and the fracture of the sprayed glassy polymers also significantly affects the deposition process.
Polymer cold spray has gained considerable attention as a novel manufacturing process. A promising aspect of this technology involves the ability to deposit uniform polymer coatings without the requirements of solvent and/or high temperature conditions. The present study investigates the interplay between shear instability, often considered to be the primary mechanism for bond formation, and fracture, as a secondary energy dissipation mechanism, collectively governing the deposition of glassy thermoplastics on similar and dissimilar substrates. A hybrid experimental-computational approach is utilized to explore the simultaneous effects of several interconnected phenomena, namely the particle-substrate relative deform ability, molecular weights, and the resultant yielding versus fracture of polystyrene particles, examined herein as a model material system. The computational investigations are based on constitutive plasticity and damage equations determined and calibrated based on a statistical data mining approach applied to a wide collection of previously reported stress-strain and failure data. Results obtained herein demonstrate that the underlying adhesion mechanisms depend strongly on the molecular weight of the sprayed particles. It is also shown that although the plastic deformation and shear instability are still the primary bond formation mechanisms, the molecular-weight-dependent fracture of the sprayed glassy polymers is also a considerable phenomenon capable of significantly affecting the deposition process, especially in cases involving the cold spray of soft thermoplastics on hard substrates. The strong interplay between molecular-weight-dependent plastic yielding and fracture in the examined system emphasizes the importance of molecular weight as a critical variable in the cold spray of glassy polymers, also highlighting the possibility of process optimization by proper feedstock selection.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据