Microstructure Evolution Behavior of Spray-Deposited 7055 Aluminum Alloy during Hot Deformation

期刊

METALS
卷 12, 期 11, 页码 -

出版社

MDPI
DOI: 10.3390/met12111982

关键词

spray deposition; 7055 aluminum alloy; dynamic recovery; dynamic recrystallization

资金

  1. National Natural Science Foundation of China
  2. Key Research and Development Program of Zhenjiang City
  3. Graduate Research and Innovation Projects in Jiangsu Province
  4. Undergraduate Innovation and Entrepreneurship Training Program of Jiangsu Province
  5. [52205421]
  6. [GY2021003]
  7. [GY2021020]
  8. [KYCX21_3453]
  9. [202210289112Y]

向作者/读者索取更多资源

The evolution behaviors of the second phase, substructure and grain of the spray-deposited 7055 aluminum alloy during hot compression were studied. Results showed that certain phases dissolved gradually while others remained unchanged. The alloy exhibited plastic instability at specific temperature and strain rate, and both partial dynamic recrystallization and continuous dynamic recrystallization were observed.
The evolution behaviors of the second phase, substructure and grain of the spray-deposited 7055 aluminum alloy during hot compression at 300 similar to 470 degrees C were studied by scanning electron microscopy (SEM), electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Results show that the AlZnMgCu phase resulting from the deposition process dissolves gradually with the increase in deformation temperature, but the Al7Cu2Fe phase remains unchanged. The plastic instability of the spray-deposited 7055 aluminum alloy occurs at 470 degrees C with a 1 similar to 5 s(-1) strain rate range. Partial dynamic recrystallization (PDRX) adjacent to the original high angle grain boundaries (HAGBs) not only occurs at 300 similar to 400 degrees C with the low strain rates ranging from 0.001 to 0.1 s(-1) but also at 450 degrees C with a high strain rate of 5 s(-1) . Continuous dynamic recrystallization (CDRX) appears at 450 degrees C with a low strain rate of 0.001 s(-1). The primary nucleation mechanism of PDRX includes the rotation of the subgrain adjacent to the original HAGBs and the subgrain boundary migration. The homogeneous misorientation increase in subgrains is the crucial nucleation mechanism of CDRX. At 300-400 degrees C, the residual coarse particle stimulated (PSN) nucleation can also be observed.