The study compares the properties of untreated and treated date palm fiber and kenaf-reinforced epoxy hybrid composite, with T-3DP7K exhibiting the best tensile properties and T-7DP3K showing superior impact properties.
This research is a comparative study of untreated and treated date palm fiber (DPF) and kenaf (KF)-reinforced epoxy hybrid composite and explores the properties of DPF. The prepared hybrid composites were characterized in terms of tensile properties, impact properties, physical behavior, water absorption, and thickness swelling. The composites were prepared by hand layup technique. Treated 30% date palm and 70% kenaf (T-3DP7K) showed the highest tensile strength (26.45 MPa) and modulus (4.54 GPa) among untreated and treated hybrid composites. The scanning electron microscope revealed the behavior of fiber and polymers and also the cause of tensile test failure. The impact strength of T-1DP1K revealed highest impact resistant (5493 J/m) among untreated and treated hybrid composites. Remarkably, alkali-treated hybrid composites reduced the water absorption and thickness swelling compared to the untreated composites. In untreated composites, higher DPF content composites showed higher moisture content and dimensional instability. Overall, we concluded that among all hybrid composites, T-3DP7K showed better tensile properties, lowest water absorption, and lowest thickness swelling, and T-7DP3K showed better impact properties.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据