In this study, flexible films of polyaniline/carbon quantum dots were fabricated using the electropolymerized approach. The films exhibited excellent electrochromic properties and demonstrated good infrared emissivity modulation performances. The integrated electrochromic device based on the fabricated films achieved dynamic conversion and showed promising applications in adaptive IR sensors and thermoregulation.
The electrochromic (EC) process is essentially an electrochemical reaction associated with the intercalation (de -intercalation) of ions to (from) the EC film. To improve the infrared emissivity modulation performances of the infrared electrochromic devices (IR-ECDs), polyaniline/carbon quantum dots (PANI/CDs) flexible films were fabricated by the electropolymerized approach in this paper. The prepared PANI/CDs porous films were exhibited and verified excellent electrochromic properties through micromorphology analysis and electro-chemical tests. The measured emittance variation (Delta e) of the prepared PANI/CDs samples are 0.41, 0.46, and 0.42 in ranges of wavelength 3-5 mu m, 8-14 mu m, and 2.5-25 mu m, respectively. In addition, for the infrared range of 2.5-25 mu m, the radiation energy can be continuously modulated from 80.77 to 241.98 W/m2 (Delta P = 161.21 W/ m2). The assembled IR-ECD based on PANI/CDs films obtains excellent IR modulation ability, that the emittance variations are 0.39, 0.41, and 0.37 in the wavelength ranges of 3-5 mu m, 8-14 mu m, and 2.5-25 mu m, respectively. The switching times of the device for the coloration and bleaching are 3.1 s and 3.7 s respectively, much shorter than that of previously reported ECDs based on PANI. Meanwhile, the developed ECD presents decent durability, as the Delta epsilon values of IR-ECD in wavelength ranges of 3-5 mu m, 8-14 mu m, and 2.5-25 mu m maintaining radio of 75%, 76%, and 68%, and current maintaining ratio of the device is above 90% after aging measurements of consec-utive 100 cycles. Furthermore, the integrated IR-ECD was proposed to achieve dynamic conversion from golden yellow to dark green in the visible light regime through precise tuning of external biasing voltage. The proposed ECD based on PANI/CDs technology is promising for the future of adaptive IR sensors and thermoregulation-related applications.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据