Calcium hexaluminate forms solid solutions with magnetic ions, allowing for the design of magnetic behavior based on composition. In this study, various synthesis methods of calcium hexaluminate with iron were investigated to determine the maximum percentage of iron that can exhibit magnetic behavior.
Calcium hexaluminate (CA6) forms a broad range of solid solutions by substitution of Al3+ with other cations such as, for example, Fe, Co, Mn, etc. Solid solutions of CA6 with magnetic ions have attracted interest because they allow designing the magnetic behavior depending on the composition of each solid solution. In this paper, we have studied materials pertaining to an area of the CaO-Al2O3-Fe2O3 ternary phase diagram that is potentially interesting, but which has not been too much explored so far. We report on various synthesis methods of calcium hexaluminate with iron in solid solution. The percentages of iron introduced have been varied in order to determine the maximum percentage of iron that can enter into solid solution in the calcium hexaluminate such that the materials obtained exhibit magnetic behavior.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据