This study determined the optimum asphalt binder contents and investigated the influence of high-viscosity modifier on the PAC-13 mixture. The laboratory tests showed that the PAC-13 mixture modified with 10% HVM-C and 0.4% polyolefin was suitable for the top layer, while the PAC-13 mixture modified with 3.3% HVM-C and 0.4% polyolefin was suitable for the bottom layer. The tested mixtures met the standard requirements for high-temperature stability, low-temperature performance, moisture sensitivity, and permeability.
Porous asphalt concrete (PAC) has the benefits of good drainage performance and excellent skid resistance. In double-layer porous pavement, the top layer ensures good pavement performance, and the bottom layer maintain the lateral drainage capacity with the air voids content. However, there is no uniform layer thickness design for double-layer porous asphalt pavement. This study determined the optimum asphalt binder contents of PAC-13 mixtures, and investigated the influence of high-viscosity modifier on the PAC-13 mixture. The laboratory properties related to filed performance were obtained, including high-temperature stability, water stability, high-temperature performance, low-temperature performance, and water permeability. The PAC-13 mixture modified with 10% high-viscosity modifier C (HVM-C) and 0.4% polyolefin was used as the mixture for the top layer, and the PAC-13 mixture modified with 3.3% HVM-C and 0.4% polyolefin was used as the mixture for the bottom layer. The optimum binder content was found to be 4.8% for top-layer PAC-13 mixture and 4.7%-4.8% for bottom-layer PAC-13 mixture. In terms of rutting resistance performance, there was an increasement of 14.6% for the dynamic stability indicator when the HVM-C content increased from 3.3% to 10%. The low-temperature performance, moisture sensitivity, and permeability of the tested mixtures met the standard requirement.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据