4.6 Article

Mechanism of titanium electrochemical oxidation via isotopic labeling, high resolution ion depth profiling, and impedance spectroscopy

期刊

ELECTROCHIMICA ACTA
卷 435, 期 -, 页码 -

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2022.141342

关键词

Anodization; Isotopic labelling; Mechanism of TiO2 growth; High-resolution depths profiling; Point defect model (PDM); Charge carrier densities

资金

  1. NSERC/CRSNG Discovery Grant [RGPIN-2020-06679, RGPIN-2018-06672]
  2. Western University

向作者/读者索取更多资源

The electrochemical oxidation mechanism of titanium was studied using isotopic labeling. The results show that the titanium oxide layer consists of two distinct regions and the carrier density decreases with the increase of voltage.
The electrochemical oxidation mechanism of titanium between 0 and 10 V vs saturated calomel reference electrode (SCE) was examined for ultra-thin Ti films sputtered onto Si(001) substrates and exposed in-situ to (H2O)-O-18, and then anodized in (D2O)-O-16. The effects of this isotopic labeling procedure were studied using medium energy ion scattering (MEIS) and nuclear reaction profiling (NRP). Both MEIS and NRP results are consistent in showing that the titanium oxide layer is composed of two distinct regions, (TiO2)-O-16/(TiO2)-O-18/Ti/Si(001) for the entire range of the formation voltages (0-10 V vs SCE). The outermost region consists entirely of O-16, and the O-18 region is always adjacent to the Ti metal. The two distinct structures observed can be consistent with both the point defect model (PDM) or high-field model (HFM), assuming the mobility of titanium cations is much higher compared to the mobility of oxygen ions. No Ti or O-18 loss into the electrolyte during anodization is detected. Linear growth rate is observed in 0-10 V range vs SCE with experimental anodization ratio of 24.5 +/- 0.6 angstrom V-1. Mott-Schottky (MS) analyses show positive slopes, indicating formation of an n-type TiO2 semiconductor, with O vacancies (or Ti interstitials) as major charge carriers in the 0-10 V range. Charge carrier densities, N-D = (0.8-5.0)x10(21) cm(-3) were calculated from Mott-Schottky analysis and were well within the range of results reported in the literature. We observe derease in the charge carrier densities above similar to 4 V vs SCE, that can be connected to defects annihilation or minor modification in the structure of the growing TiO2 film.