Understanding the Effects of Tetrahedral Site Occupancy by the Zn Dopant in Li-NMCs toward High-Voltage Compositional-Structural-Mechanical Stability via Operando and 3D Atom Probe Tomography Studies

期刊

ACS APPLIED MATERIALS & INTERFACES
卷 15, 期 1, 页码 782-794

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsami.2c15054

关键词

Zn-doped Li-NMC cathode; operando synchrotron XRD; operando stress measurement; 3D atom probe tomography; Li-ion batteries

向作者/读者索取更多资源

A new concept of blocking Ni-migration pathway by Zn-doping in Li-layered cathode materials has been proposed, leading to significant improvement in high-voltage cyclic stability.
Ni-containing layered/cation-ordered LiTMO2s (TM = transition metal) suffer from Ni-migration to the Li-layer at the unit cell level, concomitant transformation to a spinel/rock salt structure, hindrance toward Li-transport, and, thus, fading in Li-storage capacity during electrochemical cycling (i.e., repeated delithiation/lithiation), especially upon deep delithiation (i.e., going to high states-of-charge). Against this backdrop, our previously reported work [ACS Appl. Mater. Interfaces 2021, 13, 25836-25849] revealed a new concept toward blocking the Ni-migration pathway by placing Zn2+ (which lacks octahedral site preference) in the tetrahedral site of the Li-layer, which, otherwise, serves as an intermediate site for the Ni-migration to the Li-layer. This, nearly completely, suppressed the Ni-migration, despite being deep delithiated up to a potential of 4.7 V (vs Li/Li+) and, thus, resulted in significant improvement in the high-voltage cyclic stability. In this regard, by way of conducting operando synchrotron X-ray diffraction, operando stress measurements, and 3D atom probe tomography, the present work throws deeper insights into the effects of such Zn-doping toward enhancing the structural-mechanical-compositional integrity of Li-NMCs upon being subjected to deep delithiation. These studies, as reported here, have provided direct lines of evidence toward notable suppression of the variations of lattice parameters of Li-NMCs, including complete prevention of the detrimental c-axis collapse at high states-of-charges and concomitant slower-cum-lower electrode stress development, in the presence of the Zn-dopant. Furthermore, the Zn-dopant has been found to also prevent the formation of Ni-enriched regions at the nanoscaled levels in Li-NMCs (i.e., Li/Ni-segregation or structural densification) even upon being subjected to 100 charge/discharge cycles involving deep delithiation (i.e., up to 4.7 V). Such detailed insights based on direct/real-time lines of evidence, which reveal important correlations between the suppression of Ni-migration and high-voltage compositional-structural-mechanical stability, hold immense significance toward the development of high capacity and stable layered Li-TM-oxide based cathode materials for the next-generation Li-ion batteries.