关键词
silicone rubber; WO3-nanoparticles; Cs-137; Co-60; Am-241
类别
资金
- Princess Nourah bint Abdulrahman University, Riyadh, Saudi Arabia [PNURSP2022R28]
This study aimed to prepare groundbreaking silicone rubber samples by adding WO3 nanoparticles and testing their radiation shielding ability. The results showed that the silicone rubber with higher concentrations of WO3 nanoparticles exhibited better shielding performance.
Silicone rubbers are a good choice for shielding materials because of having elastic and attenuating properties as well as cost-effectiveness. Thus, the aim of this study was to prepare ground-breaking silicone rubber samples by adding WO3-nanoparticles and testing the performance of their radiation shielding ability against Cs-137, Co-60, and Am-241 gamma energy. Increasing the concentration of WO3 nanoparticles in silicone rubber (SR) led to decreasing the half-value layer (HVL) and mean free path (MFP) values determined for the samples tested. Furthermore, the values of MFP and HVL upsurged according to the enhancement of the photon energy. It is noteworthy that the prepared silicone rubber (SR) systems with 50 and 60 wt% concentrations of WO3-nanoparticles displayed lower HVL than the Bi2O3-containing silicone rubber (SR) systems. In the same way, studied silicone rubber SR-W60 represented the lowest HVL comprising iron ore containing silicone rubber.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据