The synergistic effect of polyaniline (PANI) was explored in liquid and vapour sarin (GB) exposure tests. PANI-ACF was found to have high surface area and micropore volume, leading to better adsorption performance for sarin compared to activated carbon fabric alone.
The synergistic effect of polyaniline (PANI) was explored in detail by conducting experiments with liquid and vapour sarin (GB) exposure tests. For that, different samples were prepared and breakthrough behaviour, liquid sarin elution profile and dynamic adsorption of vapour were studied at a different doping level of PANI and activated carbon fabric (PANI-ACF) was optimized to achieve optimum breakthrough behaviour. The results reveal that PANI-ACF of a surface density of 1.2-1.27 g/cm2 has a high surface area (914-980 m2/g) and micropore volume (0.20-0.22 (mL/g). Specific breakthrough volume (BTV), breakthrough time (BTT) and average breakthrough concentration rate were determined and found to be 243 L/g, 220-350 min and 0.004-0.0014 mu g h-1cm-2 respectively which is much better than only ACF. Hence, PANI reinforced ACF applies to selective adsorption of nerve agent sarin and consecutively in chemical nerve agent protection.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.0
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据