Progressive Damage Behaviour Analysis and Comparison with 2D/3D Hashin Failure Models on Carbon Fibre-Reinforced Aluminium Laminates

期刊

POLYMERS
卷 14, 期 14, 页码 -

出版社

MDPI
DOI: 10.3390/polym14142946

关键词

carbon fibre-reinforced aluminium laminates; CARALL; tensile properties; flexural properties; failure mechanism; 2D; 3D Hashin theories

资金

  1. Science and Technology Development Fund of Tianjin Education Commission for Higher Education [2021KJ099]
  2. Tianjin Technical Expert Project [20YDTPJC01890]
  3. Diversified investment fund projects of Tianjin applied basic research [2021KJ099, 21JCZDJC00710]

向作者/读者索取更多资源

This study investigates the mechanical response and failure mechanism of carbon fibre-reinforced aluminium laminates under tensile and flexural loading conditions. The 2D Hashin and 3D Hashin VUMAT models are used for finite element analysis, and the load versus deflection curves and scanning electron microscope are employed for performance evaluation. The results reveal that the failure modes include aluminium layer fracture, fibre pull-out, fracture, and matrix tensile fracture. Both the 2D Hashin and 3D Hashin models show similar predictions in terms of performance and failure modes, but the 3D Hashin model accurately reveals the failure mechanism and propagation mechanism of carbon fibre-reinforced aluminium laminates.
It is known that carbon fibre-reinforced aluminium laminate is the third generation of fibre metal materials. This study investigates the response of carbon fibre-reinforced aluminium laminates (CARALL) under tensile loading and three-point bending tests, which evaluate the damage initiation and propagation mechanism. The 2D Hashin and 3D Hashin VUMAT models are used to analyse and compare each composite layer for finite element modelling. A bilinear cohesive contact model is modelled for the interface failure, and the Johnson cook model describes the aluminium layer. The mechanical response and failure analysis of CARALL were evaluated using load versus deflection curves, and the scanning electron microscope was adopted. The results revealed that the failure modes of CARALL were mainly observed in the aluminium layer fracture, fibre pull-out, fracture, and matrix tensile fracture under tensile and flexural loading conditions. The 2D Hashin and 3D Hashin models were similar in predicting tensile properties, flexural properties, mechanical response before peak load points, and final failure modes. It is highlighted that the 3D Hashin model can accurately reveal the failure mechanism and failure propagation mechanism of CARALL.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据