4.7 Article

Assessing the fracture and fatigue resistance of nanostructured thin films

期刊

ACTA MATERIALIA
卷 239, 期 -, 页码 -

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.actamat.2022.118260

关键词

Fatigue; Thin films; Synchrotron diffraction; Physical vapor deposition; Micromechanics; Ductility; Ceramics

资金

  1. Austrian Federal Ministry for Digital and Economic Affairs
  2. National Foundation for Research, Technology and Development
  3. Christian Doppler Research Association
  4. Plansee SE
  5. Plansee Composite Materials GmbH
  6. Oerlikon Balzers
  7. Oerlikon Surface Solutions AG
  8. TU Wien Bibliothek

向作者/读者索取更多资源

This study investigates the fracture toughness and fatigue properties of thin films under various loading conditions, revealing their characteristics and possible deformation mechanisms. The findings contribute to improving the durability of coated engineering components.
Fatigue failure through sustained loading of ductile materials manifests in irreversible motion of dislocations, followed by crack initiation and growth. This contrasts with the mechanisms associated with brittle ceramics, such as nanostructured physical vapor deposited thin films, where inhibited dislocation mobility typically leads to interface-controlled damage. Hence, understanding the fatigue response of thin films from a fundamental viewpoint - including altered atomic bonds, crystal structures, and deformation mechanisms - holds the key to improved durability of coated engineering components. Here, a novel method utilizing quasi-static and cyclic-bending of pre-notched, unstrained microcantilever beams coupled with in situ synchrotron X-ray diffraction is presented to study the fracture toughness and fatigue properties of thin films under various loading conditions. Investigating a model system of sputterdeposited Cr and Cr-based ceramic compounds (CrN, CrB 2 , and Cr 2 O 3 ) demonstrates that the fatigue resistance of such thin films is limited by the inherent fracture toughness. In fact, cantilever cycling close to the critical stress intensity is sustained up to 10 7 load cycles on all materials, without inducing noticeable material damage, structural or stress-state changes. The observed variation in fracture toughness is put into context with linear-elastic fracture theory and complementary micro-pillar compression, thereby elucidating the wide range of values from as low as 1.6 +/- 0.2 MPa .,/ m for Cr 1.79 O 3 up to 4.3 +/- 0.3 MPa .,/ m for Cr 1.03 B 2 , respectively. Moreover, possible mechanisms governing the elastic-plastic deformation response of all coatings, both in quasi-static and cyclic-loading conditions, are discussed. Our findings contribute key-insights into the underlying mechanisms dictating the damage tolerance of PVD coated components by relating fatigue strength limits to fundamental material properties.(c) 2022 The Authors. Published by Elsevier Ltd on behalf of Acta Materialia Inc. This is an open access article under the CC BY license ( http://creativecommons.org/licenses/by/4.0/ )

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据