Lithium-ion battery; Silicon anode; Aging; Fast charging; Expansion; Cylindrical cells

向作者/读者索取更多资源

Silicon with high gravimetric capacity is commonly used in the anode of lithium-ion batteries to increase energy density. However, its volume change during charging and discharging processes can lead to aging. This study compares the charging behavior and degradation mechanisms of two commercial batteries with different silicon technologies, and explores the adaptation of charging protocols to improve cycling stability.
Silicon with a high gravimetric capacity of 3579 mAh g(-1) of the pure material becomes increasingly common in the anode of lithium-ion batteries to increase energy density on the full cell level. However, silicon changes its volume excessively during (de-)lithiation making it prone to aging. In commercial cells, it is typically applied either as SiOx or nano-Si in small quantities in a composite anode together with graphite. A different operation voltage window of silicon, varying quantities of silicon in the anode but also different technologies of the applied silicon materials, however, result in different aging behavior of the full cell-even if silicon content and capacities are similar on the data sheet. In this study, two commercial cylindrical cells in the 18650 format with differing silicon technologies are thus compared with a focus on their charging behavior and degradation mechanisms. One way to increase cycling stability with respect to the different silicon cell chemistries is the adaption of the charging protocols. Voltage limits as well as current have therefore been varied in this study using five different charging protocols. Their influence on the charging times and aging behavior is analyzed in great depth: dilatometer investigations of the anodes and their lithiation behavior, differential voltage investigations as well as a detailed post-mortem analysis including ICP-OES, SEM and EDX have identified silicon expansion at low full cell voltages as root aging mechanism in both cells.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据