This study investigates the effects of weft yarn diameter and pick density on the properties of surface roughness of 3/1 (Z) twill-woven fabrics. The findings suggest that weft yarn diameter and pick density have a significant impact on the surface roughness in diagonal and weft directions, but a minimal impact on the warp direction.
Purpose The purpose of this study is to investigate the effects of weft yarn diameter and pick density on the properties of surface roughness (SMD) of 3/1 (Z) twill-woven fabrics in three measurement directions weft (0 degrees), the warp (90 degrees) and the diagonal (45 degrees). Design/methodology/approach Nine 3/1 (Z) twill samples were prepared with two factors and three levels and their roughness values were measured in the weft (0 degrees), warp (90 degrees) and diagonal (45 degrees) directions of 3/1 (Z) twill fabrics using the Kawabata-FB4 instrument. Analysis of variance (ANOVA) is used to determine the effect of weft yarn diameter and pick density on SMD properties and comparisons were done in the weft (0 degrees), the warp (90 degrees) and the diagonal (45 degrees) directions. Findings From experimental analysis, weft yarn diameter and pick density affect SMD of 3/1 (Z) twill-woven fabrics in both diagonal (45 degrees) and weft (0 degrees) directions but slightly affect warp (90 degrees) direction. Maximum SMD values were observed in diagonal (45 degrees) directions and the minimum was in warp (90 degrees) directions of fabrics. Weft yarn diameter and pick density are statistically significant on SMD values of 3/1 (Z) twill-woven fabrics for three directions at a 95% confidence interval. Parameter variation in weft directions of 3/1 (Z) twill-woven fabrics also varies SMD values in three directions measurements Originality/value The findings of this study can be usually used for textile technology, industries and laboratories to create a basic understanding for measuring roughness properties of 3/1 (Z) twill fabric. It is also possible to identify the surface characterizations in different directions of measurement for their usage in some specific areas of end application like consumer goods, home textiles, technical textiles, etc.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据