This paper analyzes the degradation performance of monocrystalline silicon PV modules exposed outdoor for eleven years in Bouzareah city, northern Algeria under Mediterranean climate conditions. The results show that the PV modules suffer mainly from optical failures, leading to reductions in electrical parameters and influence on temperature coefficients.
This paper presents an analysis, assessment, and investigation of the degradation performance of the monocrystalline silicon PV modules with two glass types (Float, Textured) exposed outdoor for eleven years under Mediterranean climate conditions in northern Algeria, Bouzareah city, Algeria. In this regard, several protocol tests, experimental and measurement procedures have been developed according to IEC 61215-2 requirements in order to inspect the performance of deployed PV modules by considering their glass types. Where, they have been the subject of several PV inspections such as visual, electrical, PV characterization, and temperature coefficients and thermographic ...etc. The inspections, classifications, and statistical analysis results reveal that the deployed PV modules with two glass types suffer mainly from optical failure occurrences. The measured electrical PV parameters (P-max, I-sc, V-oc and FF) of the deployed PV modules have been reduced with annual degradation (1.04%/year, 0.5%/year, 0.3%/year, and 1.04 %/year). In the same way, the temperature coefficients have been influenced by the PV modules degradations as well. Besides, some of the deployed PV modules characteristic curves suffered from inflex point's exhibition. The thermal inspections show that the deployed PV modules regardless of their glass types caused by the inhomogeneity distribution of the optical failures are significantly affected by minor temperature mismatch. This paper investigates and discusses as well several correlation proposals between the presented PV inspections by considering multiple impacts between these inspections and the performance of the deployed PV modules with their two glass types in view to better understand the PV module degradation.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据