The effects of grain size (GS) on tensile fatigue life of nanostructured NiTi superelastic shape memory alloys (SMAs) with GS = 10 nm, 42 nm and 80 nm are investigated. Macroscopic stress-controlled tensile fatigue tests, acoustic energy measurements and fracture surface observations were performed. It is shown that low-cycle fatigue life (under sigma(max) = 450 MPa) of nanostructured NiTi polycrystalline SMA increases significantly when GS decreases from 80 nm to 10 nm. However, there is no significant effect of GS on the intermediate-cycle fatigue life (under (sigma(max) = 300 MPa). It is found that accumulated acoustic energy can be used to distinguish the three stages of fatigue: slow crack propagation, fast crack propagation and final fracture. Micro cracks were found on fracture surfaces of all GS specimens under intermediate-cycle fatigue and on fracture surfaces of 10 nm GS specimen under low-cycle fatigue, while micro voids were found in 42 nm and 80 nm GS specimens under low-cycle fatigue. The results of the paper indicate that grain refinement down to nanoscale has potential in developing high fatigue resistance SMAs. (C) 2016 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据