Dual-Wavelength Time-Resolved Photoluminescence Study of CdSe$_\text{x}$Te$_\text{1-x}$ Surface Passivation via Mg$_\text{y}$Zn$_\text{1-y}$O and Al$_\text{2}$O$_\text{3}$

期刊

IEEE JOURNAL OF PHOTOVOLTAICS
卷 12, 期 1, 页码 309-315

出版社

IEEE-INST ELECTRICAL ELECTRONICS ENGINEERS INC
DOI: 10.1109/JPHOTOV.2021.3124169

关键词

II-VI semiconductor materials; Cadmium compounds; Absorption; Zinc; Passivation; Measurement by laser beam; Charge carrier lifetime; Cadmium telluride (CdTe); CdSeTe; front interface; MgyZn1-yO (MZO); time-resolved photoluminescence (TRPL)

资金

  1. United States Department of Energy [DE-AC36-08-GO28308]
  2. Alliance for Sustainable Energy, LLC
  3. United States Office of Naval Research [IAG-16-02002]
  4. United States Department of Energy Office of Energy Efficiency and Renewable Energy Solar Energy Technologies Office [34353]

向作者/读者索取更多资源

Determining major voltage losses in CdTe-based photovoltaics is crucial, with this study finding that a Se ratio of x = 0.2 is necessary for improving carrier lifetime in the bulk. The investigation also revealed evidence of trapping at the Mg$_\text{y}$Zn$_\text{1-y}$O/CdSe$_\text{x}$Te$_\text{1-x}$ interface, indicating further work is needed for proper passivation.
Voltage loss is currently one of the biggest challenges facing cadmium telluride (CdTe) based photovoltaics. Determining the location(s) of major voltage loss within the device stack (e.g., front/back interface, grain boundaries) is therefore of primary interest. Here, we present a custom-built time-resolved photoluminescence system with two excitation wavelengths-670 (standard) and 405 nm-to probe the device stack at depths of approximately 130 and 35 nm, respectively; their comparison helps differentiate interface and bulk contributions to carrier lifetime. We apply this system to examine the passivation effect of two significant recent advances in CdTe: the incorporation of Se to form graded CdSe$_\text{x}$Te$_\text{1-x}$ and the replacement of CdS with Mg$_\text{y}$Zn$_\text{1-y}$O. It is found that x = 0.2 Se is required to obtain lifetime improvements, primarily in the bulk. Additionally, evidence for trapping at the Mg$_\text{y}$Zn$_\text{1-y}$O/CdSe$_\text{x}$Te$_\text{1-x}$ interface was observed. This indicates further work is required to sufficiently passivate the front interface.