In this study, α-Fe2O3/NiBixFe2-xO4 composite materials were synthesized by a wet chemical route, and it was found that Bi doping significantly affects the grain size, phase fraction, and magnetic properties of the nanocomposites.
Bi architecture Fe-based system shows the most extensive applications spawned from memory to optoelectronic device. With this line of understanding, we herein synthesized alpha-Fe2O3/NiBixFe2-xO4 (0 <= x <= 0.20) by sono-wave-driven wet chemical route. The grain size of the sample reduced with increasing Bi doping concentration even though the morphological features remain the same. The presence of alpha-Fe2O3 and NiFe2O4 phases in the XRD pattern confirms the formation of composite samples. Bi doping has a significant impact on controlling the phase fraction as well as magnetic properties of the nanocomposite. The nanocomposite with x = 0.20 showed a drastic reduction in saturation magnetization (more than 7 times) as compared to the un-doped sample. The alteration of coercivity and exchange bias in the nanocomposite with Bi doping is well correlated with the fraction of NiFe2O4 phase present in the corresponding sample. Moreover, Bi doping induces the deterioration in magnetic properties in the sample.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据