The purpose of this in vitro study was to evaluate the effect of different disinfection protocols on the water contact angle and microhardness of CAD-CAM PMMA materials. The results showed that both the disinfection protocol and the material type had a significant impact on the water contact angle and microhardness of the PMMA materials.
Statement of problem. Which disinfection protocol provides optimal water contact angle and microhardness for computer-aided design and computer-aided manufacturing (CAD-CAM) polymethyl methacrylate (PMMA) materials is unclear.Purpose. The purpose of this in vitro study was to evaluate the effect of different disinfection protocols (1% sodium hypochlorite, denture cleanser gel, and effervescent tablet) on the water contact angle and microhardness of different CAD-CAM PMMA denture base materials by comparing them with a heat-polymerized PMMA.Material and methods. Disk-shaped specimens (o10x2 mm) were fabricated from 3 different CAD -CAM PMMAs-AvaDent (AV), Merz M-PM (M-PM), and Polident (Poli) -and a heat-polymerized PMMA (Vynacron) (CV) (n=21). Three disinfection protocols (1% sodium hypochlorite [HC], denture cleanser gel [GEL], an effervescent tablet [TAB]) were applied to simulate 180 days of cleansing. The water contact angle and microhardness of specimens were measured before and after disinfection and compared by using a 2-way ANOVA (a=.05).Results. For water contact angle, material (P=.010) and disinfection protocol (P=.002) had a significant effect. The material (P<.001), disinfection protocol (P=.001), and their interaction (P<.001) significantly affected the microhardness after disinfection. When the condition after disinfection was compared with that before disinfection, the water contact angle increased significantly in all material-disinfection protocol pairs (P<.025), and microhardness increased significantly in all material-disinfection protocol pairs (P<.040), except for GEL-(P=.689) or TAB-applied (P=.307) AV, HC-applied M-PM (P=.219), and TAB-applied Poli (P=.159).Conclusions. The material and disinfection protocol affected the water contact angle of all tested PMMAs after disinfection, resulting in more hydrophobic surfaces for heat-polymerized or CAD-CAM PMMAs. The microhardness of heat-polymerized PMMA was less than that of all CAD-CAM PMMAs after disinfection, regardless of the protocol. (J Prosthet Dent 2023;130:787-95)

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据