Understanding the healing behavior of asphalt binder is crucial for fatigue modeling. This study compares the damage-healing behavior of various binders using the newly developed LASH procedure and proposes a simplified S-LASH procedure for efficient evaluation. The results demonstrate the impact of penetration grade and aging on healing performance and suggest critical testing conditions for reliable assessment of healing characteristics.
Understanding of the healing behavior of asphalt binder is critical for fatigue modeling of asphalt paving materials. Binder-healing characterization based on the traditional time sweep test is time-consuming. The purpose of this study was to compare the damage-healing behavior of various neat and modified asphalt binders with the newly developed linear amplitude sweep healing (LASH) procedure, followed by verification on a simplified LASH (S-LASH) procedure to alternatively estimate binder-healing characteristics with reasonable testing efficiency. Thirteen neat and modified asphalt binders (17 sample conditions) were selected and respectively analyzed with standard LASH and S-LASH. Standard LASH showed that the healing performance of neat binders with the same penetration grade generally aligns with increasing damage. For the neat binders with different penetration grades, softer binders have better healing capacity. The negative aging effect on binder healing was demonstrated. Meanwhile, the healing master curve (HMC) was effective in comparing binder-healing characteristics under prefailure conditions. The healing rate (H-R) for the tested binders basically varied from 0.1 to 0.2. Finally, mean absolute error (MAE) analysis of HMC and H-R between standard LASH and S-LASH indicated 50% S-f (damage intensity at failure) with a 900-s rest period to be a critical LASH testing condition to derive reliable healing HMC and H-R values. S-LASH is also recommended to estimate binder healing characteristic with significantly reduced testing time. (C) 2021 American Society of Civil Engineers.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据