关键词

Chemical degradation; Ethylene glycol; Bis-2-hydroxyethyl terephthalate; Poly(ethylene terephthalate); ZnO; SBA-15; Chroma

资金

  1. National Key Research and Development Program of China [2019YFC1908204]
  2. National Natural Scientific Fund of China [21878292, 21978291, 21776289, 21908232, 22178364, 22178343, NSFC22178358]
  3. International Part-nership Program of Chinese Academy of Sciences [122111KYSB20190060]
  4. K. C. Wong Education Foundation [GJTD-2018-04]
  5. Strategic Priority Research Program of Chinese Academy of Science [XDA21060300]
  6. Innovation Academy for Green Manufacture, Chinese Academy of Sciences [IAGM-2019-A06]

向作者/读者索取更多资源

By introducing a series of mesoporous catalysts, high quality BHET with good chroma was successfully prepared, achieving efficient PET degradation, and further studying the key factors influencing the reaction.
Bis(2-hydroxyethyl terephthalate) (BHET) obtained by poly(ethylene terephthalate) (PET) catalytic glycolysis often has a slight color, which results in the subsequent preparation of repolymerized PET (rPET) with a darker color. The darker rPET is unable to be utilized in a high value. In order to obtain BHET with good chroma, a series of mesoporous catalysts were proposed and synthesized. Compared with traditional catalysts, the developed catalysts have obvious advantages to obtain BHET with a good chroma. The chromaticity values of BHET obtained through ZnO/SBA-15 catalyst are 96.64, 0.16 and 1.39 (L, a and b), and the chromaticity values of rPET after polymerization are 93.69, 0.86 and 1.31. The 5% ZnO/SBA-15 catalyst displayed prominent capabilities to degrade PET into BHET. The key factors influencing the reaction were further studied. Under the conditions of reaction temperature 197 degrees C, reaction time 1 h, mass ratio of Cat./PET 5% and mass ratio of ethylene glycol (EG)/PET 4:1, the catalytic efficiency reached the optimal one where conversion of PET is 100% and yield of BHET is 91.0%. The PET degradation kinetic was studied and conforms to the first order reaction kinetics. The reaction mechanism was deduced by in situ infrared reaction and theoretical calculation. The mechanism of ester bond breaking catalyzed by ZnO/SBA-15 was proposed. Mesoporous catalyst still has excellent catalytic activity through multiple recycling. (c) 2021 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据