Catalytic graphitization of single-crystal diamond

期刊

CARBON
卷 185, 期 -, 页码 300-313

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.carbon.2021.08.082

关键词

Diamond-to-graphite transformation; Ni-catalyzed graphitization; Single crystal diamond; Atomically-resolved TEM; Electrical conductance; Electron energy loss spectroscopy

资金

  1. Austrian Science Fund (FWF) [I 2344-N36]
  2. Slovak Science and Development Funding Agency (APVV) project [APVV-16-0319]
  3. European Research Council (ERC) under the European Union [756277-ATMEN]

向作者/读者索取更多资源

The study utilizes aberration-corrected transmission electron microscopy, Raman spectroscopy, and electrical transport measurements to investigate the structural changes during nickel-catalyzed graphitization of diamond, revealing competing atomistic processes and etching mechanisms influenced by different diamond surface orientations. This research sheds light on the synthesis of graphene-on-diamond heterostructures by clarifying the etching mechanisms and the impact of diamond surface terminations.
Diamond and graphene are carbon allotropes with starkly different physical characteristics. Their combination into graphene-on-diamond heterostructures could benefit from the complementary properties of both components. Graphitization of single-crystalline diamond surfaces is a promising synthesis route, but a clear understanding of the growth of graphene or graphite from solid carbon sources is so far missing. Using aberration-corrected transmission electron microscopy, Raman spectroscopy, and electrical transport measurements, we provide detailed insight in the mechanisms of structural changes of nickel-catalyzed graphitization of diamond. We propose competing atomistic processes occurring at contact sites of diamond and Ni, depending on diamond surface terminations. One-dimensional etching process dominates on (111) diamond surfaces that remain almost atomically flat during graphitization. Two-dimensional etching of (110) and (100) diamond surfaces results in Ni drilling into the diamond substrate. Our findings also provide evidence on the reaction rates of the catalysis. The most reactive diamond surface in the (100) orientation is covered with the largest amount of well-crystallized graphite, whereas the (111) surface shows the highest stability against catalytic etching. In the latter case, only a thin disordered graphite layer is formed, yielding the lowest electric conductance. By clarifying these etching mechanisms, our results can improve the synthesis of grapheneon-diamond heterostructures. (c) 2021 The Author(s). Published by Elsevier Ltd. This is an open access article under the CC BY license (http://creativecommons.org/licenses/by/4.0/).

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据