The study characterized and compared colloidal silicon quantum dots synthesized by different methods, revealing significant differences in their photoluminescence quantum yields, primarily influenced by surface coverage and ligand type. Furthermore, analysis of the core stress on the SiQDs provided important insights into their optoelectronic performance.
The impact of colloidal silicon quantum dots (SiQDs) on next-generation light sources is promising. However, factors determining the efficiency of SiQDs, such as the photoluminescence (PL) wavelength, PL quantum yield (PLQY), and the SiQD LED performance based on the type of ligand, ligand coverage, stress, and dangling bonds, have not been quantified. Characterizing these variables would accelerate the design and implementation of SiQDs. Herein, colloidal SiQDs were synthesized by pyrolyzing hydrogen silsesquioxane and their surfaces were terminated with 1-decene by either thermal hydrosilylation (HT-SiQDs) or room-temperature hydrosilylation using PCl5 (RT-SiQD). As a result, PL, PL-excitation, and ultraviolet-visible absorption spectra were similar, but their PLQYs were significantly different: 54% (RT-SiQDs) vs 19% (HT-SiQDs). To understand their similarities and differences, surface coverages (dangling bonds, Si-H ((math)Si-H-1, =Si-H-2, and -Si-H-3), Si-O-Si, Si-C, Si-Cl) were determined. A core stress analysis established that a single ligand terminated to a SiQD bond site stretched the Si-Si bond length by 0.3%. From the two well-defined SiQDs, the PLQY and SiQD LED efficiency were attributed to four factors: low coverage of insulator ligands, the Cl ligand effect on radiative and nonradiative rates, negligible dangling bonds, and a SiQD core with low tensile stress. The PLQY of the RT-SiQDs in toluene was 80%. In addition, the 20x electroluminescence intensity difference of the LEDs originated from a 10x difference in current density and a 2x difference in Auger recombination. The concepts demonstrated here can be applied to further improve the PLQY and LED efficiencies of SiQDs with other ligands.