The study analyzed the influence of manufacturing processes on the morphological quality and mechanical behavior of multi-material metal-polymer composites joints, as well as the effects of additives on the properties of composite materials. It was found that the manufacturing process affects the polymer interface thickness and porosity, which in turn strongly influence the mechanical behavior and structural health monitoring sensitivity.
Co-cured multi-material metal-polymer composites joints are recent interesting structural materials for locally reinforcing a structure in specific areas of high structural requirements, in fibre metal laminates and lightweight high-performance structures. The influence of manufacturing processes on the morphological quality and their mechanical behaviour has been analysed on joints constituted by sol-gel treated Ti6Al4V and carbon fibre reinforced composites (CFRP). In addition, carbon nanotubes (CNT) have been added to an epoxy matrix to develop multiscale CNT reinforced CFRP, increasing their electrical conductivity and allowing their structural health monitoring (SHM). Mechanical behaviour of manufactured multi-material joints is analysed by the measurement of lap shear strength (LSS) and Mode I adhesive fracture energy (GIC) using double cantilever beam specimens (DCB). It has been proven that the addition of MWCNT improves the conductivity of the multi-material joints, even including surface treatment with sol-gel, allowing structural health monitoring (SHM). Moreover, it has been proven that the manufacturing process affects the polymer interface thickness and the porosity, which strongly influence the mechanical and SHM behaviour. On the one hand, the increase in the adhesive layer thickness leads to a great improvement in mode I fracture energy. On the other hand, a lower interface thickness enhances the SHM sensibility due to the proximity between MWCNT and layers of conductive substrates, carbon woven and titanium alloy.