This experimental study investigated the performance of sheathed cold-formed steel C-lipped wall studs with service holes under compression and bending forces. The results showed that the spacing of connectors significantly influenced the load-bearing capacity of the studs.
An experimental study of sheathed cold-formed steel C-lipped wall studs, with service holes, subjected to compression and major axis bending is presented in this paper. A total of 17 experiments were performed with both oriented strand board (OSB) and plasterboard used as sheathing and with varying connector spacing employed between the sheathing panels and the steel members. The tested specimens comprised a single 2.4 m long column sheathed on both sides and secured at the ends to top and bottom tracks. The member tests were complemented by material tests, stub column tests and initial geometric imperfection measurements. The specimens were tested in a dual-actuator rig where axial compression was applied by means of a vertical actuator through the top track, while bending was applied through the application of four lateral point loads. Eight pure compression tests with both plasterboard and OSB sheathing and with the spacing of the connectors varying between 75 mm and 600 mm were initially performed. Specimens with OSB sheathing were then tested under pure bending and combined loading. The full load-deformation responses and failure modes of the member test specimens are reported. The compressed studs connected to the plasterboard sheathing at wider spacings exhibited pull-through failure of the connectors, followed by flexural torsional buckling, while the specimens with denser connector spacings, failed by local buckling at the member ends. The OSB sheathed specimens under pure compression failed by local and distortional buckling, those under combined loading exhibited local failure at the service openings, while for those under pure bending, local buckling and stud to-track connector failure occurred. Reducing the spacing of the connectors from 600 mm to 75 mm resulted in up to 20% and 30% increases in capacity for the studs sheathed with OSB and plasterboard respectively.