4.7 Article

Siliconization elimination for SiC coated C/C composites by a pyrolytic carbon coating and the consequent improvement of the mechanical property and oxidation resistances

期刊

JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
卷 41, 期 10, 页码 5046-5055

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.jeurceramsoc.2021.04.008

关键词

Carbon; carbon composites; Silicon carbide coating; Pyrolytic carbon coating; Siliconization; Mechanical property; Oxidation resistance

资金

  1. National Natural Science Foundation of China [91860118, 51727804, 91860203]
  2. Innovation Talent Promotion Plan of Shaanxi Province for Science and Technology Innovation Team [2020TD-003]
  3. General Project (Youth) of Shaanxi Provincial Natural Science Basic Research Program [2020JQ170]

向作者/读者索取更多资源

The use of a pyrolytic carbon (PyC) coating prior to the fabrication of a silicon carbide (SiC) coating on carbon/carbon (C/C) composites helps to mitigate the negative effects of siliconization erosion, leading to an increase in flexural strength retention and better oxidation resistance. The presence of PyC coating allows for the fabrication of a compact SiC coating without silicon phase, resulting in improved performance under dynamic and static oxidation conditions at different temperatures.
Carbon/carbon (C/C) composites have a wide application as the thermal structure materials because of their excellent properties at high temperatures. However, C/C composites are easily oxidized in oxygen-containing environment, which limits their potential applications to a great degree. Silicon carbide (SiC) ceramic coating fabricated via pack cementation (PC) was considered as an effective way to protect C/C composites against oxidation. But the mechanical properties of C/C composites were severely damaged due to chemical reaction between the molten silicon and C/C substrate during the preparation of SiC coating by PC. In order to eliminate the siliconization erosion, a pyrolytic carbon (PyC) coating was pre-prepared on C/C composites by the chemical vapor infiltration (CVI) prior to the fabrication of SiC coating. Due to the retardation effect of PyC coating on siliconization erosion, the flexural strength retention of the SiC coated C/C composites with PyC coating increased from 46.27 % to 107.95 % compared with the specimen without PyC coating. Furthermore, the presence of homogeneous and defect-free PyC coating was beneficial to fabricate a compact SiC coating without silicon phase by sufficiently reacting with molten silicon during PC. Therefore, the SiC coated C/C composites with PyC coating had better oxidation resistances under dynamic (between room temperature and 1773 K) and static conditions in air at different temperatures (1773-1973 K).

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据